The Mars 2020 Perseverance Rover has landed on Mars.

by Kierstin Kaim | Feb 19, 2021

The Perseverance rover touched down at the Jezero Crater on Mars February 18, 2021. Once again, our high-temperature, HAYNES® 230® alloy was used in the descent thrusters of the Sky Crane vehicle that lowered Perseverance softly onto the Martian surface. We are proud to be a part of this historic space exploration program.