Coated Electrodes

Corrosion-resistant Alloys

Coated Electrodes* Specifications
Alloy UNS AWS/ASME AMS Other
HASTELLOY® B-3®
W80675 SFA / A 5.11 (ENiMo-10)  -
HASTELLOY® C-4
W86455 SFA / A 5.11 (ENiCrMo-7)  -
HAYNES® C-22®/122
W86022 SFA / A 5.11 (ENiCrMo-10)  -
HASTELLOY® C-276
W80276 SFA / A 5.11 (ENiCrMo-4)  -
HASTELLOY® C-2000
W86200 SFA / A 5.11 (ENiCrMo-17)  -
HASTELLOY® G-30®
W86030 SFA / A 5.11 (ENiCrMo-11)  -
HASTELLOY® G-35®
W86035 SFA / A 5.11 (ENiCrMo-22)  -
HASTELLOY® HYBRID-BC1®
N10362  A 5.11( ENiMoCr-1)
 - -
ULTIMET®
R31233  -  -

High-temperature Alloys

Coated Electrodes* Specifications
Alloy UNS AWS/ASME AMS Other
HASTELLOY® X
W86002 SFA / A 5.11 (ENiCrMo-2)  -
HAYNES® 112  W86112 SFA / A 5.11 (ENiCrMo-3)  -  625 Core
HAYNES® 117  W86117 SFA / A 5.11 (ENiCrCoMo-1)  -  617 Core
HAYNES® 182  W86182 SFA / A 5.11 (ENiCrFe-3)  -
HAYNES® 230-W  W86231 SFA / A 5.11 (ENiCrWMo-1)  - -
MULTIMET®  W73155  SFA / A 5.4 (E3155) AMS 5795 

*Other alloys available upon request.
For individual coated electrode data sheets, please click on the alloy.