Codes
HAYNES® 617 alloy
(N06617, W86117) |
ASME |
Section l |
1650°F (899°C)1 |
Section lll |
Class 1 |
- |
Class 2 |
- |
Class 3 |
- |
Section lV |
HF-300.2 |
- |
Section Vlll |
Div. 1 |
1800°F (982°C)1
Code Case 2776
1650°F (899°C)2 |
Div. 2 |
- |
Section Xll |
- |
B16.5 |
- |
B16.34 |
- |
B31.1 |
1200°F (649°C)1 |
B31.3 |
- |
1Approved material forms: Plate, Sheet, Bar, Forgings, seamless pipe/tube
2Approved material forms: Bolting