Guided Bend Test Results

1/2 inch (12.7) Plate Weldments (GTAW) Using Alloy W Filler

Base Materials Bend Radius Results
188/ MULTIMET® 2t No Cracks
625/ 718 2t No Cracks
304 SS/ Carbon Steel 2t No Cracks