HAYNES® 625 alloy
(N06625, W86112) |
ASME |
Section l |
Grade 1
1100ºF (593ºC)1
Cold Case 2632
1200ºF (650ºC)2
Grade 2
1100ºF (593ºC)3
Code Case 1935
1000ºF (538ºC)3 |
Section lll |
Class 1 |
Grade 1
800ºF (427ºC)3 |
Class 2 |
Grade 1
800ºF (427ºC)4 |
Class 3 |
Grade 1
800ºF (427ºC)4 |
Section lV |
HF-300.2 |
- |
Section Vlll |
Div. 1 |
Grade 1
1200ºF (649ºC)1
Grade 2
1600ºF (871ºC)3
1200ºF (649ºC)5 |
Div. 2 |
Grade 1
800ºF (427ºC)5
Code Case 2468
800ºF (427ºC)6 |
Section Xll |
Grade 1
650ºF (343ºC)1
Grade 2
650ºF (343ºC)7 |
B16.5 |
1200°F (649°C)8 |
B16.34 |
1200°F (649°C)6 |
B31.1 |
1200°F (649°C)1 |
B31.3 |
1200°F (649°C)6 |
MMPDS
|
6.3.3
|
1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
2Plate, Sheet, welded pipe/tube
3Plate, Sheet, Bar, seamless pipe/tube
4Plate, Sheet, Bar, Forgings, welded pipe/tube, seamless pipe/tube
5Bolting
6Plate, Sheet, Bar, Forgings, seamless pipe/tube
7Plate, Sheet, Bar, seamless pipe/tube, Bolting
8Plate, Forgings